釩鈦炮泥 -- 由于鐵口區(qū)域長期受渣鐵的侵蝕局部受傷,造成爐底溫度過高,水溫差過大等問題,制約著高爐順行,經(jīng)過專家團隊科研公關研制出釩鈦炮泥有效的解決上述問題。我公司生產(chǎn)的釩鈦炮泥塑性高,通過釩鈦的逐步累積達到縮小溫差,降低爐缸區(qū)域溫度,達到養(yǎng)爐護爐的作用。
Due to the long-term local damage caused by iron slag erosion in the iron mouth area, which caused problems such as excessively high furnace bottom temperature and excessively large water temperature, restricting the blast furnace to go forward. The vanadium-titanium cannon mud developed by the expert team's scientific research and public relations effectively solved the above problems. The product has high plasticity, which can reduce the temperature difference through the gradual accumulation of vanadium and titanium, reduce the temperature of the hearth area, and achieve the role of furnace maintenance and furnace protection.
項目 |
化學組成% Chem.comp |
耐壓強度Mpa Crushing strength |
線變化率Mpa Linder change |
體積密度g/cm3 Bulk density
|
|||
Al2O3 |
Sic+C |
TiO2+V2O5 |
200℃×24h |
1350℃×3h |
1350℃×3h |
1350℃×3h |
|
HXPN-HI |
≥50 |
≥18 |
≥10 |
≥3.5 |
≥10 |
±1.5 |
≥1.8 |
備注 |
此技術參數(shù)僅供參考,針對高爐的使用效果需要研究其冶煉產(chǎn)物和操作方式,爐況予以調(diào)整。 This indicator is for reference only. For the use effect of the blast furnace, its smelting products and operation methods need to be studied, and the furnace conditions are adjusted |